Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG13 BK00102 - PA6-GF63 - BASF

Material Data Center offers the following functions for Ultramid® B3WG13 BK00102:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Ultramid® B3WG13 BK00102 is a 63% glass filled, injection molding, high modulus Polyamid designed to have high strength and stiffness for metal replacement applications. It also has excellent moldability and outstanding surface appearance.

Applications:
Potential applications are mirror brackets, fuel lids, gas-assisted steering wheel inserts, ski bindings and bike rack clamps.
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 22400 / - MPa ISO 527
破壊応力 235 / - MPa ISO 527
破壊ひずみ 2 / - % ISO 527
シャルピー衝撃強さ, +23°C 90 / - kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 90 / - kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 15 / - kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 13 / - kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 220 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 214 / * °C ISO 75-1/-2
1.5mm厚さでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 1.5 / * mm -
Yellow Card 可用 はい / * - -
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 3.0 / * mm -
Yellow Card 可用 はい / * - -
その他の特性.乾燥/調湿単位テスト基準
密度 1740 / - kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Processing humidity ≤0.03 % -
樹脂温度 300 - 320 °C -
金型温度 80 - 95 °C -
機能
 粘度せん断速度. , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
 せん断応力-せん断速度. , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
 応力-ひずみ. , Ultramid® B3WG13 BK00102 (乾燥), PA6-GF63, BASF
 応力-ひずみ. , Ultramid® B3WG13 BK00102 (調湿), PA6-GF63, BASF
 割線弾性率−ひずみ. , Ultramid® B3WG13 BK00102 (乾燥), PA6-GF63, BASF
 割線弾性率−ひずみ. , Ultramid® B3WG13 BK00102 (調湿), PA6-GF63, BASF
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット., 黒
特殊な特性.
熱安定化.
領域別の利用可能性
北アメリカ.
その他の情報
村遜速揃
PREPROCESSING
Max. Water content: 0.03%
Although Product is supplied in sealed containers, drying is recommended in applications requiring optimum surface aesthetics. A dehumidifying or desiccant dryer operating at 80 °C (176 °F) is recommended. Drying time is dependent on moisture level.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.

PROCESSING
Melt Temperature 300-320 °C (572-608 °F)
Mold Temperature 80-95 °C (176-203 °F)
Injection and Packing Pressure 35-125 bar (500-1500psi)
Rear Zone 275-300 °C (527-572 °F)
Center Zone 285-310 °C (545-590 °F)
Front Zone 300-325 °C (572-617 °F)
Nozzle 300-325 °C (572-617 °F)

This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics arecritical, a mold surface temperature of 80-95 °C (176-203 °F) is required.

Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage.

Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.